Description
Performance:
It is used for adding chromium or grain refinement in aluminum alloy melting, adding temperature is low, the loss of chromium is low.
2. Add temperature: above 730℃.
3. The amount of this product added: according to the actual calculation and test to determine.
4. Adding method: heat up to the required temperature, remove scum, put the product into aluminum liquid, melt it, mix it evenly, sample analysis, and pour it after the composition is qualified.
It is used for adding chromium or grain refinement in aluminum alloy melting, adding temperature is low, the loss of chromium is low.
Usage:
1. Bake and dry before use.2. Add temperature: above 730℃.
3. The amount of this product added: according to the actual calculation and test to determine.
4. Adding method: heat up to the required temperature, remove scum, put the product into aluminum liquid, melt it, mix it evenly, sample analysis, and pour it after the composition is qualified.
Shape and packing:
Each W.: Around 8 kg.
Packing: 1000 kgs/pallet, wrapped with heat shrinkage film.